dc.contributor.author | Zeren, Doğuş | - |
dc.contributor.author | Güden, Mustafa | - |
dc.date.accessioned | 2017-10-23T07:44:23Z | |
dc.date.available | 2017-10-23T07:44:23Z | |
dc.date.issued | 2017-05 | |
dc.identifier.citation | Zeren, D., and Güden, M. (2017). The increased compression strength of an epoxy resin with the addition of heat-treated natural nano-structured diatom frustules. Journal of Composite Materials, 51(12), 1681-1691. doi:10.1177/0021998316669855 | en_US |
dc.identifier.issn | 0021-9983 | |
dc.identifier.issn | 0021-9983 | - |
dc.identifier.issn | 1530-793X | - |
dc.identifier.uri | http://doi.org/10.1177/0021998316669855 | |
dc.identifier.uri | http://hdl.handle.net/11147/6404 | |
dc.description.abstract | Natural diatom frustules composing nanometer size silica particles were heat-treated at temperatures between 600 and 1200℃ for 2 h and used as filler/reinforcing agent (15 wt%) in an epoxy resin. The opal structure of as-received natural diatom frustules was transformed into cristobalite after the heat-treatment above 900℃. The epoxy resin test samples reinforced with heat-treated and as-received frustules and neat epoxy test samples were compression tested at the quasi-static strain rate of 7 × 10−3 s−1. The results showed that the inclusion of the frustules heat-treated at 1000℃ increased the compressive yield strength of the resin by 50%, while the addition of the diatom frustules heat-treated above and below 1000℃ and the as-received frustules increased the strength by ∼25% and 16%, respectively. The heat treatment above 1000℃ decreased the surface area of the frustules from 8.23 m2 g−1 to 3.46 m2 g−1. The cristobalite grains of the frustules heat-treated at 1000℃ was smaller than 100 nm, while the grain size increased to ∼500 nm at 1200℃. The increased compressive stresses of the resin at the specific heat treatment temperature (1000℃) were ascribed to nano size crystalline cristobalite grains. The relatively lower compressive stresses of the epoxy resin filled with frustules heat-treated above 1000℃ were attributed to the micro-cracking of the frustules that might be resulted from higher density of the cristobalite than that of the opal and accompanying reduction of the surface area and the surface pore sizes that might impair the resin-frustule interlocking and intrusion. | en_US |
dc.language.iso | en | en_US |
dc.publisher | SAGE Publications Inc. | en_US |
dc.relation.ispartof | Journal of Composite Materials | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Compression | en_US |
dc.subject | Deformation and fracture | en_US |
dc.subject | Diatomite | en_US |
dc.subject | Frustules | en_US |
dc.subject | Polymeric composites | en_US |
dc.title | The increased compression strength of an epoxy resin with the addition of heat-treated natural nano-structured diatom frustules | en_US |
dc.type | Article | en_US |
dc.authorid | TR114204 | en_US |
dc.authorid | TR114738 | en_US |
dc.institutionauthor | Zeren, Doğuş | - |
dc.institutionauthor | Güden, Mustafa | - |
dc.department | İzmir Institute of Technology. Mechanical Engineering | en_US |
dc.department | İzmir Institute of Technology. Materials Science and Engineering | en_US |
dc.identifier.volume | 51 | en_US |
dc.identifier.issue | 12 | en_US |
dc.identifier.startpage | 1681 | en_US |
dc.identifier.endpage | 1691 | en_US |
dc.identifier.wos | WOS:000401035100002 | en_US |
dc.identifier.scopus | 2-s2.0-85019097289 | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.identifier.doi | 10.1177/0021998316669855 | - |
dc.relation.doi | 10.1177/0021998316669855 | en_US |
dc.coverage.doi | 10.1177/0021998316669855 | en_US |
dc.identifier.wosquality | Q3 | - |
dc.identifier.scopusquality | Q2 | - |
item.fulltext | With Fulltext | - |
item.grantfulltext | open | - |
item.languageiso639-1 | en | - |
item.openairecristype | http://purl.org/coar/resource_type/c_18cf | - |
item.cerifentitytype | Publications | - |
item.openairetype | Article | - |
crisitem.author.dept | 03.10. Department of Mechanical Engineering | - |
Appears in Collections: | Materials Science and Engineering / Malzeme Bilimi ve Mühendisliği Mechanical Engineering / Makina Mühendisliği Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection WoS İndeksli Yayınlar Koleksiyonu / WoS Indexed Publications Collection |
CORE Recommender
SCOPUSTM
Citations
5
checked on Nov 15, 2024
WEB OF SCIENCETM
Citations
6
checked on Nov 9, 2024
Page view(s)
302
checked on Nov 18, 2024
Download(s)
388
checked on Nov 18, 2024
Google ScholarTM
Check
Altmetric
Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.