Please use this identifier to cite or link to this item:
https://hdl.handle.net/11147/2217
Full metadata record
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Demir, Hasan | - |
dc.contributor.author | Balköse, Devrim | - |
dc.contributor.author | Ülkü, Semra | - |
dc.date.accessioned | 2016-10-12T08:19:08Z | |
dc.date.available | 2016-10-12T08:19:08Z | |
dc.date.issued | 2006-05 | |
dc.identifier.citation | Demir, H., Balköse, D., and Ülkü, S. (2006). Influence of surface modification of fillers and polymer on flammability and tensile behaviour of polypropylene-composites. Polymer Degradation and Stability, 91(5), 1079-1085. doi:10.1016/j.polymdegradstab.2005.07.012 | en_US |
dc.identifier.issn | 0141-3910 | |
dc.identifier.issn | 0141-3910 | - |
dc.identifier.uri | http://doi.org/10.1016/j.polymdegradstab.2005.07.012 | |
dc.identifier.uri | http://hdl.handle.net/11147/2217 | |
dc.description.abstract | An intumescent system consisting of ammonium polyphosphate (APP) as an acid source and blowing agent, pentaerythritol (PER) as a carbonific agent and natural zeolite (clinoptilolite, Gördes II) as a synergistic agent was used in this study to enhance flame retardancy of polypropylene (FR-PP). Zeolite was incorporated into flame retardant formulation at four different concentrations (1, 2, 5, and 10 wt%) to investigate synergism with the flame retardant materials. Filler content was fixed at 30 wt% of total amounts of flame retardant PP composites. Zeolite and APP were treated with two different coupling agents namely, 3-(trimethoxysilyl)-1-propanethiol and (3-aminopropyl)-triethoxysilane for investigation of the influence of surface treatments on mechanical properties and flame retardant performance of composites. Maleic anhydride grafted polypropylene (MAPP) was used for making polypropylene hydrophilic. Flammability of FR-PP composites was measured by the determination of limiting oxygen index (LOI). The LOI values reached to a maximum value of 41% for mercapto silane treated APP:PER (2:1) PP composite containing 5 wt% zeolite. The tensile strength of composites was increased by the addition of MAPP and elongation at break of composites was increased with silane treatments. | en_US |
dc.language.iso | en | en_US |
dc.publisher | Elsevier Ltd. | en_US |
dc.relation.ispartof | Polymer Degradation and Stability | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.subject | Fillers | en_US |
dc.subject | Coupling agents | en_US |
dc.subject | Flame retardant-polypropylene | en_US |
dc.subject | Intumescent | en_US |
dc.subject | Mechanical properties | en_US |
dc.subject | Polypropylene | en_US |
dc.title | Influence of surface modification of fillers and polymer on flammability and tensile behaviour of polypropylene-composites | en_US |
dc.type | Article | en_US |
dc.authorid | TR103536 | en_US |
dc.institutionauthor | Demir, Hasan | - |
dc.institutionauthor | Balköse, Devrim | - |
dc.institutionauthor | Ülkü, Semra | - |
dc.department | İzmir Institute of Technology. Chemical Engineering | en_US |
dc.identifier.volume | 91 | en_US |
dc.identifier.issue | 5 | en_US |
dc.identifier.startpage | 1079 | en_US |
dc.identifier.endpage | 1085 | en_US |
dc.identifier.wos | WOS:000236076400012 | en_US |
dc.identifier.scopus | 2-s2.0-31444448107 | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.identifier.doi | 10.1016/j.polymdegradstab.2005.07.012 | - |
dc.relation.doi | 10.1016/j.polymdegradstab.2005.07.012 | en_US |
dc.coverage.doi | 10.1016/j.polymdegradstab.2005.07.012 | en_US |
local.message.claim | 2022-06-09T17:11:01.003+0300 | * |
local.message.claim | |rp02671 | * |
local.message.claim | |submit_approve | * |
local.message.claim | |dc_contributor_author | * |
local.message.claim | |None | * |
dc.identifier.wosquality | Q1 | - |
dc.identifier.scopusquality | Q1 | - |
item.fulltext | With Fulltext | - |
item.grantfulltext | open | - |
item.languageiso639-1 | en | - |
item.openairecristype | http://purl.org/coar/resource_type/c_18cf | - |
item.cerifentitytype | Publications | - |
item.openairetype | Article | - |
crisitem.author.dept | 03.02. Department of Chemical Engineering | - |
crisitem.author.dept | 03.02. Department of Chemical Engineering | - |
crisitem.author.dept | 03.02. Department of Chemical Engineering | - |
Appears in Collections: | Chemical Engineering / Kimya Mühendisliği Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection WoS İndeksli Yayınlar Koleksiyonu / WoS Indexed Publications Collection |
CORE Recommender
SCOPUSTM
Citations
80
checked on Nov 15, 2024
WEB OF SCIENCETM
Citations
65
checked on Nov 16, 2024
Page view(s)
282
checked on Nov 18, 2024
Download(s)
610
checked on Nov 18, 2024
Google ScholarTM
Check
Altmetric
Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.