Title: Microstructural Investigation of Discarded NdFeB Magnets After Low-Temperature Hydrogenation
Authors: Habibzadeh, Alireza
Kucuker, Mehmet Ali
Cakir, Oznur
Gokelma, Mertol
Keywords: Hydrogen decrepitation
Magnet-to-magnet recycling
Nd-rich phase
HPMS
Publisher: Springer
Abstract: Due to continuously increasing demand and limited resources of rare-earth elements (REEs), new solutions are being sought to overcome the supply risk of REEs. To mitigate the supply risk of REEs, much attention has recently been paid to recycling. Despite the more common recycling methods, including hydrometallurgical and pyrometallurgical processes, hydrogen processing of magnetic scrap (HPMS) is still in the development stage. Magnet-to-magnet recycling via hydrogenation of discarded NdFeB magnets provides a fine powder suitable for the production of new magnets from secondary sources. One of the crucial aspects of HPMS is the degree of recovery of the magnetic properties, as the yield efficiency can easily reach over 95%. The amount, morphology, and distribution of the Nd-rich phase are the key parameters to achieve the excellent performance of the magnet by isolating the matrix grain. Therefore, a better insight into the microstructure of the matrix grains and the Nd-rich phase before and after hydrogenation is essential. In this study, a low-temperature hydrogenation process in the range of room temperature to 400 degrees C was conducted as the first step to recycle NdFeB magnets from discarded hard disk drives (HDDs), and the hydrogenated powder was characterized by electron microscopy and X-ray diffraction. The results show that there are three different morphologies of the Nd-rich phase, which undergo two different transformations through oxidation and hydride formation. While at lower temperatures (below 250 degrees C) the degree of pulverization is higher and the experimental evidence of hydride formation is less clear, at higher temperatures the degree of pulverization decreases. The formation of neodymium hydride at higher temperatures prevents further oxidation of the Nd-rich phase due to its high stability.
Description: Habibzadeh, Alireza/0000-0003-1567-0755
URI: https://doi.org/10.1007/s40831-024-00873-8
https://hdl.handle.net/11147/14686
ISSN: 2199-3823
2199-3831
Appears in Collections:Scopus İndeksli Yayınlar Koleksiyonu / Scopus Indexed Publications Collection
WoS İndeksli Yayınlar Koleksiyonu / WoS Indexed Publications Collection

Show full item record



CORE Recommender

Google ScholarTM

Check




Altmetric


Items in GCRIS Repository are protected by copyright, with all rights reserved, unless otherwise indicated.