The effect of strain rate on the compressive deformation behavior of a sintered Ti6Al4V powder compact
(Elsevier, 2008)
The high strain rate (220–550 s−1) and quasi-static (0.0016 s−1) compression deformation behavior of a sintered Ti6Al4V powder compact was investigated. The compact was prepared using atomized spherical particles (100–200 ...
Processing and compression testing of Ti6Al4V foams for biomedical applications
(Springer, 2009)
Open cell Ti6Al4V foams (60% porosity) were prepared at sintering temperatures between 1,200 and 1,350 °C using ammonium bicarbonate particles (315–500 μm) as space holder. The resulting cellular structure of the foams ...