    • Organotin compounds as PVC stabilizers 

      Arkış, Esen (Wiley, 2008-09)
      When poly(vinyl chloride) is fabricated, it passes between rollers (calendars) at about 200 ◦C, which causes elimination of some HCl at allylic defects in the polymer, as shown below (Figure 3.3.1). Furthermore, the released ...